THERMAL LAB · MA-09 · MATERIALS
Lithium cells in the cold
A lithium-ion cell is a chemical device, and chemistry slows in the cold. Capacity falls, voltage sags under load, and charging below freezing can damage the cell permanently. A thermal system that depends on a battery has to manage the battery's temperature too.
What happens as a cell cools
The electrolyte thickens and ions move more slowly. Internal resistance rises. Under load, more voltage is lost inside the cell, so the device reaches its cutoff voltage sooner and reports the pack empty while charge remains.
| Cell temperature | Typical effect on usable capacity |
|---|---|
| 20 to 25 °C (68 to 77 °F) | Rated capacity |
| 0 °C (32 °F) | Noticeably reduced, more so at high load |
| -10 °C (14 °F) | Substantially reduced |
| -20 °C (-4 °F) | A fraction of rated capacity for many consumer cells |
The exact figures depend on cell chemistry and on how hard the cell is being driven. Warm the cell again and most of the capacity returns.
Charging is the real hazard
Discharging a cold cell is inefficient. Charging one is harmful. Below about 0 °C (32 °F), lithium can deposit as metal on the anode in place of entering it. This plating reduces capacity permanently and can create internal faults. Well-designed packs refuse to charge when cold. Cheap ones may not.
Design responses
- Carry the battery warm. Inside the outer layer, near the body, a pack stays in its working range in weather far below freezing.
- Insulate the pack. A cell under load warms itself a little. Insulation keeps that heat.
- Size for the cold. Plan capacity on what the pack delivers at the temperature it will see.
- Reduce the load. A cold cell copes better with a modest steady draw than with peaks.
- Heat the pack where needed. Equipment left outside may need a small heater to bring cells up to temperature before use or charging.
Self-regulating heaters and cold starts
A PTC heating element draws its highest current when cold, exactly when a cold battery is least able to supply it. The combination can trip a pack's protection at start-up. It has to be tested from a cold soak. See cold conditions testing.
Reading capacity labels
Capacity is printed in mAh at the cell voltage. Convert to watt-hours for comparison: amp-hours multiplied by volts. Air transport rules are written in watt-hours for this reason.
Knowledge background: why batteries die in the cold, batteries in extreme cold and how battery pack heaters work.